Abstract:
The objective of this study was to investigate the strength of In-Ceram and IPS Empress 2 with different thickness of core and veneer ratio by means of biaxial flexural strength (BFS). A total 100 disc samples, diameter 15+-0.5 mm. with 1.2+-0.005mm. in thickness, were fabricated following manufacturer's recommendations. The samples were divided into 10 groups (n=10, each), group 1-5 were In-Ceram (Vita ,Zahnfabrik,BadSakingen, Germany ) with veneer porcelain vitadur alpha (Vita Zahnfabrik,BadSakingen, Germany) by group 1 in ratio 1.2 : 0 , group 2 in ratio 0.8 : 0.4, group 3 in ratio 0.6 : 0.6 , group 4 in ratio 0.4 : 0.8 , group 5 in ratio 0 :1.2 and group 6-10 were IPS Empress 2 (Vivadent, Schaan, Liechtenstein) with veneer porcelain IPS Eris (Vivadent, Schaan, Liechtenstein) by group 6 in ratio 1.2 : 0, group 7 in ratio 0.8 : 0.4, group 8 in ratio 0.6 : 0.6, group 9 in ratio 0.4 : 0.8 , group 10 in ratio 0 :1.2. All samples were subjected to BFS testing following ISO 6872: 1995. All tests were carried out on the Instron 5583 (Instron, Canton, MA, USA) with crosshead speed of 1.0 mm/ min. The means+-SD of each groups were 433.06+-68.37 MPa for Group 1, 338.90+-22.56 MPa for Group 2, 294.43+-15.19 MPa for Group 3, 259.94+-14.53 MPa for Group 4, 56.59+-10.54 MPa for Group 5, 288.31+-44.64 MPa for Group 6, 246.34+-28.16 MPa for Group 7, 258.63+-27.87 MPa for Group 8, 226.59+-26.37 MPa for Group 9, and 68.56+-5.52 MPa for Group 10. ANOVA and Tamhane's Test revealed that the BFS of In- ceram alone was significantly higher than In-Ceram combined with veneer porcelain as well as decreasing of strength when the thickness of core was decreased respectively (p<0.05). For IPS Empress 2, the BFS of IPS Empress 2 alone was not significantly different from IPS Empress 2 combined with veneer porcelain with any core:veneer ratio (p<0.05). It was concluded that core and veneer thickness ratio affect the BFS of In-Ceram but not for IPS Empress 2